HOME > Product > High performance Admixtures

High performance Admixtures

Name : WINFLOW-GR(High performance AE high range water reducer)

Type : Retarders Type

Download : 다운로드

WINFLOW-GR    High performance AE high range water reducer (Retarders Type) KSF 2560

AE high range water reducer helps produce high performance concrete that improves the reliability of concrete structures. It helps provide high fluidity that minimizes heat of hydration, stiffening, drying shrinkage, and the impact of construction conditions during placement, and provides external resistance and durability in long term.



USAGE
*
High-strength high-performance concrete structures
*
Hot weather concrete
*
Dam concrete and Mass Concrete
*
Fields where concrete casting is delayed and the concrete requires low heat

* Commonly used in ready-mixed concrete plants


DOSAGE
*
The amount used is generally 0.5% to 2.5% by weight of the cement, but consultation is required since the amount necessary may vary, depending on the formulation and application of the concrete.



ADVANTAGES
*
Provides mechanical and chemical robustness through copolymer molecules with double chain structures.
*
Effective in the prevention of joints by helping adjust the setting time of concrete in summer.

* Heat of hydration and cracking are suppressed and durability is increased.

* By minimizing variations in slump, concrete of a high level of quality is possible.


PROPERTIES
*
Appearance  : Dark brown liquid
*
Specific gravity   : 1.200±0.05 (20℃)
*
pH       : 7.0±3.0


Packing : 250kg/drum, 1TON/drum, Tank Lorry




 

MixingDesign




 Class

Gravel
Size(mm)

 W/C(%)

S/A(%)

 Unit weight (kg/㎥)

 W

 C

 S

 G

 AD

 PLAIN

 25

 65.6

 48.5

210

 320

 855

 915

 

 WINFLOW-GR

 25

 51.6

 47.5

 165

320

 856

 954

3.84



TestResults



 Test Item

 KSF2560

 PLAIN

 WINFLOW-GR

 Admixture dosage (%)

 -

 -

 1.2

 Water Reduction (%)

 18≤

 -

21.4

 Bleeding (%)

 70≥

100 

55.3

 Setting Time
(Hr : Min)

Initial

 +90~+240

 0

+105

Final

+240≥

 0

+110

 Compressive strength ratio(%)

3Day

 135≤

 100

150

7Day

 125≤

 100

142

28Day

 115≤

 100

146

Elongation (%)

 110≥

 -

104

Relative dynamic modulus of elasticity (%)

 80≤

 -

98.1

 Time dependent change (initial→60min)

 Slump(㎜)

 60≥

 180

 185 → 155

 Air(%)

 ±1.5

 1.7

 4.6 → 4.2

 

Length change test           : Water curing for 7 days (20±2) and moist curing for 6 months (Temperature 20±2, Humidity 60±5%)

Freeze-Thaw Resistance test        : Specimen Temp. (4℃ → -18,  -184) 200 cycles

이전  다음 